Реферат:
The patterns of formation of carbon from n-hexane on an alumino-platinum catalyst (1 Wt. % Pt/γ-A2O3) were studied by derivatography, electron microscopy, and x-ray phase analysis methods, and the reasons for its increased stability to coking on modification with tin were analyzed.
Библиографическая ссылка:
Chesnokov V.V.
, Buyanov R.A.
, Pakhomov N.A.
, Zaikovskii V.I.
Reasons for Increase in the Stability to Coking of an Alumino-Platinum Catalysts on Modification with Tin
Kinetics and Catalysis. 1991. V.32. N6-2. P.1337-1341. WOS РИНЦ
Reasons for Increase in the Stability to Coking of an Alumino-Platinum Catalysts on Modification with Tin
Kinetics and Catalysis. 1991. V.32. N6-2. P.1337-1341. WOS РИНЦ
Оригинальная:
Чесноков В.В.
, Буянов Р.А.
, Пахомов Н.А.
, Зайковский В.И.
Причины повышения коксоустойчивости алюмоплатинового катализатора при модифицировании оловом
Кинетика и катализ. 1991. Т.32. №6. С.1494-1499. РИНЦ
Причины повышения коксоустойчивости алюмоплатинового катализатора при модифицировании оловом
Кинетика и катализ. 1991. Т.32. №6. С.1494-1499. РИНЦ
Даты:
Поступила в редакцию: | 19 апр. 1990 г. |
Опубликована в печати: | 1 нояб. 1991 г. |
Идентификаторы БД:
Web of science | WOS:A1991JB14200020 |
РИНЦ | 31189873 |
Цитирование в БД:
Пока нет цитирований