Design of Anodes for IT SOFC: Effect of Complex Oxide Promoters and Pd on Activity and Stability in Methane Steam Reforming of Ni/YSZ (ScSZ) Cermets
Научная публикация
Общее |
Язык:
Английский,
Жанр:
Статья (Full article),
Статус опубликования:
Опубликована,
Оригинальность:
Оригинальная
|
Конференция |
2006 MRS Fall Meeting: Symposium AA - Solid-State Ionics-2006
27 нояб. - 1 дек. 2006
,
Boston, MA
|
Журнал |
Materials Research Society Symposium Proceedings
ISSN: 0272-9172
|
Вых. Данные |
Год: 2006,
Том: 972,
Страницы: 205-210
Страниц
: 6
DOI:
10.1557/PROC-0972-AA03-06
|
Авторы |
Sadykov Vladislav A.
1
,
Mezentseva Natalia V.
2
,
Bunina Rimma V.
2
,
Alikina Galina M.
2
,
Lukashevich Anton I.
2
,
Rogov Vladimir A.
2
,
Moroz Ella M.
2
,
Zaikovskii Vladimir I.
2
,
Ishchenko Arcady
2
,
Bobrenok Oleg F.
3
,
Smirnova Alevtina
4
,
Irvine John
5
,
Vasylyev Oleksandr
6
|
Организации |
1 |
Heterogeneous catalysis, Boreskov Institute of Catalysis, pr. Lavrentieva, 5, Novosibirsk, 630090, Russian Federation
|
2 |
Boreskov Institute of Catalysis, Novosibirsk, 630090, Russian Federation
|
3 |
Institute of Thermophysics SB RAS, Novosibirsk, 630090, Russian Federation
|
4 |
University of Connecticut, Storrs, CT, 06269
|
5 |
University of St Andrews, Fife, KY169ST, United Kingdom
|
6 |
Institute for Problems of Materials Science, Kyiv, 03142, Ukraine
|
|
Информация о финансировании (2)
1
|
Президиум СО РАН
|
95
|
2
|
North Atlantic Treaty Organization
|
SfP-980878
|
Effect of fluorite-like or perovskite-like complex oxide promoters and Pd on the performance of Ni/YSZ and Ni/ScSZ cermets in methane steam reforming or selective oxidation by O2 into syngas at short contact times was studied. Spatial uniformity of dopants distribution in composites was controlled by TEM combined with EDX, while the lattice oxygen mobility and reactivity was elucidated by CH4 and H2 TPR. Oxide promoters allow to operate even at stoichiometric H2O/CH4 ratio by suppressing coke deposition through modification of Ni surface, while doping by Pd ensures reasonable performance at moderate (∼550 °C) temperatures required for Intermediate–Temperature Solid Oxide Fuel Cells (IT SOFC).