Zirconium-Containing Compositions with a Component Ratio Characteristic of the Garnet Structure: Physicochemical and Catalytic Properties Научная публикация

Журнал Kinetics and Catalysis
ISSN: 0023-1584 , E-ISSN: 1608-3210
Вых. Данные Год: 2000, Том: 41, Номер: 6, Страницы: 816-825 Страниц : 10 DOI: 10.1023/A:1026685422492
Ключевые слова Oxidation; Precipitation; Physical Chemistry; Surfactant; Hydrocarbon
Авторы Ivanova A.S. 1 , Mikhan’ M.V. 1 , Alikina G.M. 1 , Litvak G.S. 1 , Moroz E.M. 1 , Burgina E.B. 1
Организации
1 Boreskov Institute of Catalysis, Siberian Division, Russian Academy of Sciences, Novosibirsk, 630090, Russia

Реферат: The possibility for the formation of garnet in the Mn-Fe-Zr-O and Ca-Sm-Zr-O catalytic systems, derived by the precipitation of the corresponding salts, was investigated. The physicochemical and catalytic properties of these systems in the complete oxidation of hydrocarbons were tested. In the Mn-Fe-Zr-O system, garnet was crystallized at 860°-920°C, for which probable cation distribution was estimated to be {Zr2.5 4+Mn0.5 2+} [Mn2 2+](Fe2.5 3+ Mn0.5 3+)O12. In the Ca-Sm-Zr-O system, the perovskite CaZrO3, pyrochlore Sm2Zr2O7, and CaO were formed at 900°-1200°C, but no compounds with garnet structures were observed. The systems had surface areas of 300-450 sq m/g at ≤450°C and polydisperse distribution of pores over sizes. The addition of surfactants during component mixing caused an increase in the overall pore volume and mechanical strength of the systems. The Mn-Fe-Zr and Ca-Sm-Zr compositions proved active for the complete oxidation of hydrocarbons. The activity of the Mn-Fe-Zr-O sample, calcined at a higher temperature than other catalysts, was comparable to that of other samples. A switch from a catalyst with 1-2 mm grains to granules did not lead to a considerable decrease in activity. The use of the Mn-Fe-Zr-O catalyst in the form of rings was favorable for the more efficient use of the active component compared with known catalysts. distribution of pores over sizes. The introduction of surfactants at the stage of component mixing enables an increase in the overall pore volume and mechanical strength of these systems. The Mn–Fe–Zr and Ca–Sm–Zr compositions are active catalysts for the complete oxidation of hydrocarbons
Библиографическая ссылка: Ivanova A.S. , Mikhan’ M.V. , Alikina G.M. , Litvak G.S. , Moroz E.M. , Burgina E.B.
Zirconium-Containing Compositions with a Component Ratio Characteristic of the Garnet Structure: Physicochemical and Catalytic Properties
Kinetics and Catalysis. 2000. V.41. N6. P.816-825. DOI: 10.1023/A:1026685422492 WOS Scopus РИНЦ РИНЦ CAPlusCA OpenAlex
Оригинальная: Иванова А.С. , Михань М.В. , Аликина Г.М. , Литвак Г.С. , Мороз Э.М. , Бургина Е.Б.
Цирконийсодержащие композиции с соотношением компонентов, характерным для структуры граната: физико-химические и каталитические свойства
Кинетика и катализ. 2000. Т.41. №6. С.897-906. Scopus РИНЦ
Даты:
Поступила в редакцию: 30 июл. 1999 г.
Опубликована в печати: 1 нояб. 2000 г.
Идентификаторы БД:
Web of science: WOS:000166250600018
Scopus: 2-s2.0-0043282235
РИНЦ: 43191205 | 44930693
Chemical Abstracts: 2001:30621
Chemical Abstracts (print): 134:243205
OpenAlex: W348416894
Цитирование в БД:
БД Цитирований
Web of science 1
OpenAlex 1
Альметрики: