High-Temperature XRD Investigation of Spinel Mn1.5Al1.5O4 Decomposition Full article
Conference |
12th European Powder Diffraction Conference 27-30 Aug 2010 , Darmstadt |
||||||
---|---|---|---|---|---|---|---|
Journal |
Zeitschrift für Kristallographie
ISSN: 0044-2968 |
||||||
Output data | Year: 2011, Volume: 226, Number: 1, Pages: 325-330 Pages count : 6 DOI: 10.1524/9783486991321-054 | ||||||
Tags | high-temperature XRD, spinel, catalyst structure | ||||||
Authors |
|
||||||
Affiliations |
|
Abstract:
This article describes a study of behaviour of cubic Mn1.5Al1.5O4 spinel during heating and cooling under air. High-temperature XRD and TEM were used to investigate structure transformations and sample microstructure. XRD data show spinel decomposition during cooling and heating under air at 500-700oC. The products of decomposition consist of nanocrystalline tetragonal phase (with particle size of 20 nm) and cubic spinel (50 nm). Cu-bic spinel composition changes by various ways on the initial step during the heating and cooling. Thus, the structure mechanisms of decomposition are different. But the final de-composition products are the same.
Cite:
Bulavchenko O.
, Tsybulya S.
, Gerasimov E.
, Cherepanova S.
, Afonasenko T.
, Tsyrulnikov P.
High-Temperature XRD Investigation of Spinel Mn1.5Al1.5O4 Decomposition
Zeitschrift für Kristallographie. 2011. V.226. N1. P.325-330. DOI: 10.1524/9783486991321-054 РИНЦ OpenAlex
High-Temperature XRD Investigation of Spinel Mn1.5Al1.5O4 Decomposition
Zeitschrift für Kristallographie. 2011. V.226. N1. P.325-330. DOI: 10.1524/9783486991321-054 РИНЦ OpenAlex
Identifiers:
Elibrary: | 21810966 |
OpenAlex: | W2495346963 |
Citing:
Пока нет цитирований