Joining Ti-Based Metallic Glass and Crystalline Titanium by Magnetic Pulse Welding Научная публикация

Журнал Journal of Non-Crystalline Solids
ISSN: 0022-3093 , E-ISSN: 1873-4812
Вых. Данные Год: 2022, Том: 597, Номер статьи : 121912, Страниц : 8 DOI: 10.1016/j.jnoncrysol.2022.121912
Ключевые слова Magnetic-pulse welding; High-velocity impact; Metallic glass composite; Synchrotron X-ray diffraction; Small angle X-ray scattering; Transmission electron microscopy
Авторы Lazurenko D.V. 1 , Ivannikov А.А. 2 , Anisimov A.G. 3 , Popov N.S. 2 , Dovzhenko G.D. 1,4 , Bataev I.A. 1 , Emurlaev K.I. 1 , Ogneva T.S. 1 , Golovin E.D. 1
Организации
1 Novosibirsk State Technical University, Karl Marks av. 20, 630073 Novosibirsk, Russia
2 National Research Nuclear University MEPhI (Moscow Engineering Physics Institute), Kashirskoye Shosse, 31, 115409 Moscow, Russia
3 Lavrentiev Institute of Hydrodynamics SB RAS, Lavrentiev av., 15, 630090 Novosibirsk, Russia
4 Boreskov Institute of Catalysis SB RAS, Lavrentiev av., 5, 630090 Novosibirsk, Russia

Информация о финансировании (2)

1 Российский научный фонд 22-23-00953
2 Министерство науки и высшего образования Российской Федерации (с 15 мая 2018) 075-15-2021-698

Реферат: Due to low thermal stability and limited critical size, metallic glasses (MGs) are frequently considered for reinforcing composites. The production technology of composites should provide the minimum heat input to preserve the disordered structure of MGs. In this study, the solid-state magnetic pulse welding (MPW) was used to join crystalline titanium and Ti-based MG. The amorphous structure of the MG layer after MPW was confirmed by synchrotron X-ray radiation diffraction (XRD), ultra-small-angle X-ray scattering (uSAXS), and transmission electron microscopy (TEM). Crystalline particles were found only in the mixing zones subjected to the strongest heating during welding. The average size of the crystalline precipitates was about 25 nm, and their phase composition corresponded to a-Ti. In addition to Ti particles, titanium oxides and nitrides could form at the interface of Ti and MG layers during MPW.
Библиографическая ссылка: Lazurenko D.V. , Ivannikov А.А. , Anisimov A.G. , Popov N.S. , Dovzhenko G.D. , Bataev I.A. , Emurlaev K.I. , Ogneva T.S. , Golovin E.D.
Joining Ti-Based Metallic Glass and Crystalline Titanium by Magnetic Pulse Welding
Journal of Non-Crystalline Solids. 2022. V.597. 121912 :1-8. DOI: 10.1016/j.jnoncrysol.2022.121912 WOS Scopus РИНЦ CAPlus OpenAlex
Даты:
Поступила в редакцию: 13 июн. 2022 г.
Принята к публикации: 6 сент. 2022 г.
Опубликована online: 13 сент. 2022 г.
Опубликована в печати: 1 дек. 2022 г.
Идентификаторы БД:
Web of science: WOS:000876392300009
Scopus: 2-s2.0-85137751400
РИНЦ: 57556646
Chemical Abstracts: 2022:2394639
OpenAlex: W4296311918
Цитирование в БД:
БД Цитирований
Scopus 10
Web of science 9
OpenAlex 9
Альметрики: