Oxygen Dissolution in Polycrystalline Palladium at O2 Pressures of 0.1 to 100 Pa Full article

Journal Kinetics and Catalysis
ISSN: 0023-1584 , E-ISSN: 1608-3210
Output data Year: 2013, Volume: 54, Number: 1, Pages: 106-118 Pages count : 13 DOI: 10.1134/S0023158413010114
Tags Palladium; Oxide Film; Subsurface Layer; Oxide Film Surface; Palladium Oxide
Authors Salanov A.N. 1 , Suprun E.A. 1
Affiliations
1 Boreskov Institute of Catalysis, Siberian Branch, Russian Academy of Sciences, Novosibirsk, 630090, Russia

Abstract: Oxygen dissolution in polycrystalline palladium Pd(poly) at O2 pressures ( PO2) of 0.1 to 100 Pa and a temperature of 600 K has been investigated by temperature-programmed desorption. The dissolution process under these conditions includes O2 chemisorption on the oxide film surface, the insertion of Oads atoms under the oxide layer, and their diffusion into the subsurface layers of palladium. During chemisorption, a structure ensuring that the Oads coverage of the surface increases with increasing PO2 forms on the surface of the oxide film. This is favorable for Oads penetration through the oxide film and increases the amount of absorbed oxygen. The Oads coverage of the surface calculated via the Langmuir equation at an O2 desorption activation energy of E des = 125 kJ/mol correlates with the number of absorbed oxygen monolayers (n). At n ≥ 1, oxygen absorption by Pd(poly) is due to the diffusion of O atoms in the palladium lattice. After the accumulation of 14–18 oxygen monolayers in the subsurface layers of palladium, oxygen absorption practically stops depending on PO2. Thus, the acceleration of oxygen dissolution in palladium is due to the formation of the surface oxide film and the increase in the Oads coverage of this film, which facilitates the insertion of Oads atoms into the subsurface layers of palladium.
Cite: Salanov A.N. , Suprun E.A.
Oxygen Dissolution in Polycrystalline Palladium at O2 Pressures of 0.1 to 100 Pa
Kinetics and Catalysis. 2013. V.54. N1. P.106-118. DOI: 10.1134/S0023158413010114 WOS Scopus РИНЦ ANCAN OpenAlex
Original: Саланов А.Н. , Супрун Е.А.
Растворение кислорода в поликристаллическом палладии при давлениях О2 от 0.1 до 100 Па
Кинетика и катализ. 2013. Т.54. №1. С.111-125. DOI: 10.7868/S0453881113010115 РИНЦ OpenAlex
Dates:
Submitted: Mar 26, 2012
Published print: Jan 1, 2013
Published online: Feb 5, 2013
Identifiers:
Web of science: WOS:000314534800013
Scopus: 2-s2.0-84873361108
Elibrary: 20427192
Chemical Abstracts: 2013:197850
Chemical Abstracts (print): 158:516052
OpenAlex: W2032912741
Citing:
DB Citing
Web of science 3
Scopus 3
Elibrary 3
OpenAlex 3
Altmetrics: