Sciact
  • EN
  • RU

Size Effect in the Oxidation–Reduction Processes of Platinum Particles Supported onto Silicon Dioxide Full article

Journal Kinetics and Catalysis
ISSN: 0023-1584 , E-ISSN: 1608-3210
Output data Year: 2015, Volume: 56, Number: 6, Pages: 801-809 Pages count : 9 DOI: 10.1134/S0023158415060129
Tags hydrogen, NO + O2, platinum oxides, supported model catalysts, X-ray photoelectron spectroscopy
Authors Smirnov M.Yu. 1 , Kalinkin A.V. 1 , Vovk E.I. 1,2 , Bukhtiyarov V.I. 1
Affiliations
1 Boreskov Institute of Catalysis, Siberian Branch, Russian Academy of Sciences, Novosibirsk, 630090 Russia
2 Chemistry Department, Bilkent University, 06800 Bilkent, Ankara, Turkey

Funding (1)

1 Russian Science Foundation 14-23-00146

Abstract: The interaction of the Pt/SiO2 model catalysts as thin films on the surface of tantalum supports with a mixture of NO + O2 (1 : 1) was studied by Xray photoelectron spectroscopy. The pressure of the reaction mixture was varied from 6 to 64 mbar, and the temperature was varied from room temperature to 500°C. Two types of the catalysts, in which the Pt/Si atomic ratios were ~0.1 and ~0.3 (0.1Pt/SiO2 and 0.3Pt/SiO2, respectively) according to the XPS data, were studied. In 0.1Pt/SiO2, the particles of platinum predominantly had a size from 1 to 2.5 nm; a wide Pt particle size distribution in a range from 1 to 15 nm with a maximum at ~4 nm was characteristic of 0.3Pt/SiO2. The interaction of all of the samples with NO + O2 at room temperature led to the dissolution of oxygen atoms in the bulk of platinum metal particles. As the reaction temperature was increased, PtOx platinum oxide particles were formed: from small Pt particles in 0.1Pt/SiO2 at 300°C and from larger particles in 0.3Pt/SiO2 at 400–500°C. It was established that the reactivity of platinum oxide particles toward hydrogen also depended on the particle size. The small particles of platinum oxide were converted into platinum metal under the action of hydrogen (16 mbar) at 300°C. The coarse particles of PtOx in the samples of 0.3Pt/SiO2 were reduced much more easily starting with room temperature.
Cite: Smirnov M.Y. , Kalinkin A.V. , Vovk E.I. , Bukhtiyarov V.I.
Size Effect in the Oxidation–Reduction Processes of Platinum Particles Supported onto Silicon Dioxide
Kinetics and Catalysis. 2015. V.56. N6. P.801-809. DOI: 10.1134/S0023158415060129 WOS Scopus РИНЦ AN OpenAlex
Original: Смирнов М.Ю. , Калинкин А.В. , Вовк Е.И. , Бухтияров В.И.
Размерный эффект в процессах окисления–восстановления частиц платины, нанесенных на диоксид кремния
Кинетика и катализ. 2015. Т.56. №6. С.791-799. DOI: 10.7868/S0453881115060131 РИНЦ OpenAlex
Files: Full text from publisher
Dates:
Submitted: Jan 14, 2015
Published print: Nov 1, 2015
Published online: Nov 24, 2015
Identifiers:
Web of science: WOS:000365450000013
Scopus: 2-s2.0-84948399465
Elibrary: 24974251
Chemical Abstracts: 2015:1918999
OpenAlex: W2221594446
Citing:
DB Citing
Web of science 14
Scopus 15
OpenAlex 16
Altmetrics: