Formation of Aluminum Hydroxide During Aging Full article
Journal |
Kinetics and Catalysis
ISSN: 0023-1584 , E-ISSN: 1608-3210 |
||
---|---|---|---|
Output data | Year: 1976, Volume: 17, Number: 2, Pages: 415-421 Pages count : 7 | ||
Authors |
|
||
Affiliations |
|
Abstract:
Aluminum hydroxide formed at pH 6 and 20° by hydrolysis of Al4O2(OH)7NO3. Dependences of degree of hydrolysis and crystallization and the surface area on time have a stationary part diminishing with increase of pH. The surface area is connected with the degree of crystallization and the small surface area is caused by sintering of primary particles.
Cite:
Dzis'ko V.A.
, Ivanova A.S.
, Vishnyakova G.P.
Formation of Aluminum Hydroxide During Aging
Kinetics and Catalysis. 1976. V.17. N2. P.415-421. WOS РИНЦ
Formation of Aluminum Hydroxide During Aging
Kinetics and Catalysis. 1976. V.17. N2. P.415-421. WOS РИНЦ
Original:
Дзисько В.А.
, Иванова А.С.
, Вишнякова Г.П.
Формирование гидроокиси алюминия при старении
Кинетика и катализ. 1976. Т.17. №2. С.483-490. РИНЦ
Формирование гидроокиси алюминия при старении
Кинетика и катализ. 1976. Т.17. №2. С.483-490. РИНЦ
Dates:
Submitted: | Jun 26, 1974 |
Identifiers:
Web of science | WOS:A1976CP42700013 |
Elibrary | 30626126 |
Citing:
DB | Citing |
---|---|
Web of science | 3 |