Formation of the Pore Structure of Oxide Vanadium–Titanium–Phosphorus Catalysts in the Course of Thermal Treatment Full article

Journal Kinetics and Catalysis
ISSN: 0023-1584 , E-ISSN: 1608-3210
Output data Year: 2004, Volume: 45, Number: 5, Pages: 702-707 Pages count : 6 DOI: 10.1023/B:KICA.0000044982.61360.d0
Tags Oxide; Titanium; Physical Chemistry; Phosphorus; Catalysis
Authors Gavrilov V.Y. 1 , Zenkovets G.A. 1 , Zalomaeva O.V. 1 , Tsybulya S.V. 1
Affiliations
1 Boreskov Institute of Catalysis, Siberian Division, Russian Academy of Sciences, Novosibirsk, 630090 Russia

Abstract: The effect of the conditions of the thermal treatment of vanadium–titanium–phosphorus catalysts on the formation of the pore structure and phase composition was studied. It was found that the optimum doping of catalysts with phosphorus (5 wt % P2O5) was favorable for retention of the high dispersity of primary particles up to 450°C. The main change in the texture of the catalysts occurred within the range of micropores and mesopores with D < 10 nm. The formation of the coarsely dispersed well-crystallized phase of a vanadium–titanium–phosphorus compound was detected.
Cite: Gavrilov V.Y. , Zenkovets G.A. , Zalomaeva O.V. , Tsybulya S.V.
Formation of the Pore Structure of Oxide Vanadium–Titanium–Phosphorus Catalysts in the Course of Thermal Treatment
Kinetics and Catalysis. 2004. V.45. N5. P.702-707. DOI: 10.1023/B:KICA.0000044982.61360.d0 WOS Scopus РИНЦ ANCAN OpenAlex
Original: Гаврилов В.Ю. , Зенковец Г.А. , Заломаева О.В. , Цыбуля С.В.
Формирование пористой структуры оксидных ванадий-титан-фосфорных катализаторов при термообработке
Кинетика и катализ. 2004. Т.45. №5. С.742-747. РИНЦ
Dates:
Submitted: Mar 28, 2003
Published print: Sep 1, 2004
Identifiers:
Web of science: WOS:000224886200012
Scopus: 2-s2.0-6044220005
Elibrary: 18244064
Chemical Abstracts: 2004:840796
Chemical Abstracts (print): 142:436530
OpenAlex: W2034910115
Citing:
DB Citing
Web of science 2
Scopus 1
Elibrary 1
OpenAlex 2
Altmetrics: