Influence of Carbon-Nanotube Diameters on Composite Dielectric Properties Научная публикация
Журнал |
Physica Status Solidi (A) Applications and Materials (after 2004)
ISSN: 1862-6300 , E-ISSN: 1862-6319 |
||||||
---|---|---|---|---|---|---|---|
Вых. Данные | Год: 2013, Том: 210, Номер: 11, Страницы: 2491-2498 Страниц : 8 DOI: 10.1002/pssa.201329254 | ||||||
Ключевые слова | chemical vapor deposition, electrical properties, polymer-matrix composites, thermal analysis | ||||||
Авторы |
|
||||||
Организации |
|
Информация о финансировании (5)
1 | European Commission | 266529 FP7-INCO-2010-6 BY-NANOERA |
2 | European Commission | 610875 FP7-PEOPLE-2013-IRSES NAmiceMC |
3 | European Commission | 318617 FP7-PEOPLE-2012-IRSES FAEMCAR |
4 | Министерство образования и науки Российской Федерации | 8748 |
5 | Белорусский республиканский фонд фундаментальных исследований | F12Lat-007 |
Реферат:
The dielectric properties of polymethylmetacrylate (PMMA) composites filled with CVD made multiwalled carbon nanotubes (MWCNT) of different mean outer diameters (d ∼ 9 nm and 12–14 nm) were investigated in the temperature range from 300 to 420 K and in a wide frequency range (20 Hz to 1 MHz). Below the percolation threshold the temperature dependence of the complex dielectric permittivity of the investigated composites is mainly caused by β relaxation in pure PMMA matrix and the dielectric permittivity is found to be higher in composites with thicker nanotubes. The activation energy of β relaxation increases with carbon nanotube concentration. The percolation threshold is lower in composites with both thinner and oxidized carbon nanotubes. The established influence of both the MWCNT mean outer diameter and their oxidation on the broadband dielectric characteristics can be exploited for the production of effective low-cost electromagnetic and/or antistatic coatings working at different temperatures.
Библиографическая ссылка:
Macutkevic J.
, Kuzhir P.
, Paddubskaya A.
, Shuba M.
, Banys J.
, Maksimenko S.
, Kuznetsov V.L.
, Mazov I.N.
, Krasnikov D.V.
Influence of Carbon-Nanotube Diameters on Composite Dielectric Properties
Physica Status Solidi (A) Applications and Materials (after 2004). 2013. V.210. N11. P.2491-2498. DOI: 10.1002/pssa.201329254 WOS Scopus РИНЦ
Influence of Carbon-Nanotube Diameters on Composite Dielectric Properties
Physica Status Solidi (A) Applications and Materials (after 2004). 2013. V.210. N11. P.2491-2498. DOI: 10.1002/pssa.201329254 WOS Scopus РИНЦ
Даты:
Поступила в редакцию: | 15 апр. 2013 г. |
Принята к публикации: | 31 июл. 2013 г. |
Опубликована online: | 23 авг. 2013 г. |
Опубликована в печати: | 1 нояб. 2013 г. |
Идентификаторы БД:
Web of science | WOS:000330245200038 |
Scopus | 2-s2.0-84888204828 |
РИНЦ | 21891414 |
Chemical Abstracts | 2013:1312704 |
Chemical Abstracts (print) | 160:111562 |
OpenAlex | W1960158663 |