Sciact
  • EN
  • RU

Fenton Degradation of Sulfanilamide in the Presence of Al,Fe-Pillared Clay: Catalytic Behaviour and Identification of the Intermediates Научная публикация

Журнал Journal of Hazardous Materials
ISSN: 0304-3894 , E-ISSN: 1873-3336
Вых. Данные Год: 2015, Том: 293, Страницы: 21-29 Страниц : 9 DOI: 10.1016/j.jhazmat.2015.03.038
Ключевые слова Degradation intermediates, Hydrogen peroxide, Oxidation, Pillared clays, Sulfanilamide
Авторы Khankhasaeva Sesegma Ts. 1,2 , Dambueva Darima V. 1 , Dashinamzhilova Elvira Ts. 1 , Gil Antonio 3 , Vicente Miguel A. 4 , Timofeeva Maria N. 5,6,7
Организации
1 Baikal Institute of Nature Management SB RAS, Str. Sakh’yanova 8, 670047 Ulan-Ude, Russian Federation
2 Buryat State University, Str. Smolina 24a, 670000 Ulan-Ude, Russian Federation
3 Department of Applied Chemistry, Public University of Navarra, 31006 Pamplona, Spain
4 Department of Inorganic Chemistry, University of Salamanca, Salamanca, Spain
5 Boreskov Institute of Catalysis SB RAS, Prospekt Akad. Lavrentieva 5, 630090 Novosibirsk, Russian Federation
6 Novosibirsk State University, St. Pirogova 2, 630090 Novosibirsk, Russian Federation
7 Novosibirsk State Technical University, Prospekt K. Marksa 20, 630092 Novosibirsk, Russian Federation

Информация о финансировании (5)

1 Федеральное агентство научных организаций России V.44.2.12.
2 Федеральное агентство научных организаций России V.46.5.1.
3 Ministry of Economic Affairs and Digital Transformation MAT2013-47811-C2-1-R, MAT2013-47811-C2-2-R
4 Министерство образования и науки Российской Федерации
5 Ministry of Economic Affairs and Digital Transformation

Реферат: Liquid phase catalytic degradation of sulfanilamide with H2O2 was carried out in the presence of Fe,Al/M-pillared clay (Fe,Al/M-MM, M = Na+, Ca2+and Ba2+) as heterogeneous Fenton type catalyst. Fe,Al/M-MMswere prepared by swelling of layered aluminosilicate (90–95 wt.% montmorillonite) from a bed locatedin Mukhortala (Buryatia, Russia) in Na+, Ca2+and Ba2+forms by means of the exchange of these cationswith bulky Fe,Al-polyoxocations prepared at Al/Fe = 10/1 and OH/(Al + Fe) = 2.0, and then calcinated at500◦C. XRD method and chemical analysis demonstrated that the rate of crystalline swelling was depen-dent on the interlayer cations and decreased in the order: Fe,Al-/Na-MM > Fe,Al/Ca-MM > Fe,Al/Ba-MM.It was found that the catalytic properties of Fe,Al/M-MMs depended on the type of exchangeable cations
Библиографическая ссылка: Khankhasaeva S.T. , Dambueva D.V. , Dashinamzhilova E.T. , Gil A. , Vicente M.A. , Timofeeva M.N.
Fenton Degradation of Sulfanilamide in the Presence of Al,Fe-Pillared Clay: Catalytic Behaviour and Identification of the Intermediates
Journal of Hazardous Materials. 2015. V.293. P.21-29. DOI: 10.1016/j.jhazmat.2015.03.038 WOS Scopus РИНЦ CAPlusCA PMID OpenAlex
Даты:
Поступила в редакцию: 20 нояб. 2014 г.
Принята к публикации: 12 мар. 2015 г.
Опубликована online: 19 мар. 2015 г.
Опубликована в печати: 1 авг. 2015 г.
Идентификаторы БД:
Web of science: WOS:000355043000004
Scopus: 2-s2.0-84925440324
РИНЦ: 24019638
Chemical Abstracts: 2015:486928
Chemical Abstracts (print): 162:453778
PMID (PubMed): 25819990
OpenAlex: W1965510716
Цитирование в БД:
БД Цитирований
Web of science 55
Scopus 60
РИНЦ 59
OpenAlex 63
Альметрики: